be free of separating and adhesion-reducing substances, e.g. dust, stillage, grease, rubber abrasion, (Larger defects and cracks must be repaired in advance using suitable products from the SCHOMBURG range.) The material temperature during the mixing process should be approx. +15°C. Do not mix the mixed material process in the delivery container! Pour the mixture into a clean mixing bucket and stir carefully again. Intermediate compaction is absolutely necessary in accordance with the specified material layer thicknesses. In the case of a two-layer design, the fresh primer is added to the second layer after the first layer has hardened After curing, the unbound quartz sand portion must be carefully removed before a rolling/leveling coating, scratch filler or screed is applied. T.